Cooper River Bridge Figures 3.1 - 3.10
|
|
Figure
|
Description
|
Thumbnail
|
|
3.1
|
View of "built-up" box shape. Note the stiffener which is installed to seal end of box for corrosion protection.
|
|
|
3.2
|
Built up H shape. At this point the three plates have been installed in the welding jig.
|
|
|
3.3
|
Preheating is used for welding high strength materials to avoid brittleness. Note the automated equipment.
|
|
|
3.4
|
Welding operation by the submerged arc weld method.
|
|
|
3.5
|
Preheating and welding in one operation.
|
|
|
3.6
|
Before being shipped out to the bridge site, the trusses are assembled in the shop to check for dimensional tolerances.
|
|
|
3.7
|
Painting of steel for corrosion protection occurs prior to erection.
|
|
|
3.8
|
More painting of the truss.
|
|